Acid Bench 80

From LNF Wiki
Jump to navigation Jump to search
Acid Bench 80
Acid 80.jpg
Equipment Details
Technology Process Technology
Materials Restriction Broad
Chemicals Used

Acetic Acid (C2H4O2)

Aluminum Etch

Buffered HF (BHF)

Hydrofluoric acid (HF)

Chromium Etch

Hydrochloric acid (HCl)

Hydrogen peroxide (H2O2)

Gold Etch

Nanostrip

Nitric acid (HNO3)

Phosphoric Acid (H3O4P)

Sulfuric acid (H2SO4)
Equipment Manual
Overview System Overview
Operating Procedure SOP
Maintenance Maintenance



The Acid Bench 80 is a wet bench used for working with acids, mostly for etching and cleaning of samples that have had metals and/or polymers on them. It is considered a Metals class tool, so wafers with metal are allowed in the bench with some restrictions. It is intended for use with mixed materials and all substrate sizes up to 6 inches with the main focus being on piece parts.

Announcements

  • [7/2024] A programmable timer module has been installed in this tool to aid users in timed processing. Please create a Helpdesk ticket if you would like to be shown how to program it.

Capabilities

This bench is mostly used for beaker processing with a storage tank for leaving samples soaking overnight. You may leave a chemical soaking in the bath for up to 48 hours.

LNF Provided Chemicals

System overview

Hardware details

  • Bottle wash
  • Gooseneck sink
  • QDR
  • Overnight storage tank

Substrate requirements

  • Wafer Size: any
  • Wafer type: metals allowed

Material restrictions

Below is a list of approved materials for the tool. Approved means the material is allowed in the tool under the classification described above. If a material is not listed, please create a helpdesk ticket or email info@lnf.umich.edu for any material requests or questions.


Supported processes

There are several processes for this tool supported by the LNF, which are described in more detail on the Processes page.

In addition to these, this tool has a number of user-created recipes for etching a wide variety of materials. Some of these recipes are documented on Acid Bench 80 user processes. If you are curious if your material can be processed in this tool, please contact the tool engineers via the helpdesk ticket system.

Standard operating procedure

A reader friendly version of the SOP can be found with the link here: SOP Widget text will go here.

Checkout procedure

  1. Take the General Wet Bench Training, if you haven't already.
  2. Read through this page and the Standard Operating Procedure above.
  3. Fill out Acid Bench Process Request Form Form. You will need to fill this out for each bench you plan on using.
  4. Practice with your mentor or another authorized user until you are comfortable with tool operation.
    1. If your mentor is not an authorized user or you do not know of an authorized user that can train you, you may request training from LNF Staff.
  5. Score 100% on this quiz: 1440 Acid Bench Training Quiz.
  6. Request a checkout session with a tool engineer via the helpdesk ticket system. If this checkout is successful, the engineer will authorize you on the tool.