===Thermal Oxidation===
{{main|Thermal oxidation}}
Thermal oxidation is used to grow very high quality silicon dioxide on silicon. By exposing silicon to oxygen at very high temperatures (~1000 C), the silicon and oxygen react and form silicon dioxide. Thermal oxidation is typically used to grow silicon dioxide for MOS transistor gates.
==Figures of merit==