===Etch/Dep Rate===
Etch rate is feature size dependent - smaller features will etch slower than larger ones. Bulk etch rate is approximately 2500 Å/min. The etch exhibits minimal [[loading]] effect.
 
* Thermal oxide: 2450 Å/min
* GSI Oxide 200C: 2550 Å/min