====Stress Adjustment Unit====
*The stress adjustment unit is used to adjust change the resistance in a capacitance/resistance path circuit to ground of the chamber.
**Users can adjust the dial before their runs.
**Typically adjustments below 25 will lead to plasma instability issues so the vendor does not recommend going below that point.