Changes

Jump to navigation Jump to search

Sputter deposition

185 bytes added, 3 years ago
<!--*[[Germanium|Germanium(Ge)]]-->
*[[Iron|Iron(Fe)]]
*[[Indium Tin Oxide|Indium Tin Oxide(ITO)]]
*[[Molybdenum|Molybdenum(Mo)]]
*[[Nickel|Nickel (Ni)]]
*[[Platinum|Platinum(Pt)]]
*[[Silicon nitride|Silicon nitride(SiN)]]
*[[Silver|Silver(Ag)]]
*[[Tantalum|Tantalum(Ta)]]
*[[Tantalum Oxide|Tantalum Oxide(Ta2O5)]]
*[[Titanium|Titanium(Ti)]]
*[[Titanium Oxide|Titanium Oxide(TiO2)]]
<!--*[[Titanium dioxide|Titanium dioxide(TiO2)]]-->
OnlineAccess, PhysicalAccess, Staff, StoreManager, StoreUser