49 bytes removed, 3 years ago
no edit summary
==Limitations==
This process should not be run below 25 mTorr since To remove the tool has difficulty stabilizing photoresist a pure HBr process ~20 sec dip in that pressure regime100:1 HF is necessary before nanostrip.