===Uniformity===
Uniformity measures the variation in thickness across a substrate and is usually expressed as a percentage. Typically: (Thickness Max - Thickness Min)/(2*Thickness Average).
Uniformity is typically set by the material being deposited and the geometry of the system: throw distance, substrate rotation and deposition angle.