SPR 220 7.0

No change in size, 2 years ago
This could be potentially be caused by UV exposure and simultaneous heating during the DRIE step creating N2 bubble.
After develop
*#Flood Expose Sample for 45 sec on MA/BA6*#Wait >1hr*#DRIE
===Resist peeling during DRIE===