===Deposition Equipment===
*Tools in the LNF for depositing this material.Evaporation
** [[Angstrom Engineering Evovac Evaporator]]
** [[Cooke Evaporator]]
** [[SJ-20 Evaporator]]
*Sputtering
** [[PVD 75 Proline]]
===Etching Equipment===
==Processes==
===Deposition Processes===
* List of technologies for depositing this material and relevant process information specific to this material associated with this equipment/type of process.[[Electron beam evaporation]]* [[Sputter deposition]]
===Etching Processes===
* Nickel can be etched with [[Piranha Etch]] (380 nm/min), dilute [[Aqua Regia]] (100 nm/min)
*[[Plasma etching]]