LAM 9400/Processes/LNF Aluminum

27 bytes added, 1 year ago
*PMMA: 73.4 nm/min
*ZEP: 49.4 nm/min
*GaN (N-Polar): 18.7 nm/min
=== SF<sub>6</sub> Ash ===