<!-- Describe the checkout procedure for the tool. For example: -->
# Complete a [[Lithography training session]]. If you have already completed this for another tool, you do not need to complete it again.
# Read through the [https://drive.google.com/file/d/0B3k-qgz56T_4a0JrTjR5N004d2s/view?usp=sharing Standard Operating Procedure]User Manual above.
# Practice with your mentor or another authorized user until you are comfortable with tool operation.
# Complete Accurately complete the [https://docs.google.com/a/lnf.umich.edu/forms/d/1L5TToo8m1ZaTqTK5p8UJ6gEcPR_8UFawA21pygwi_34/viewform SOP quiz]. You may retake as necessary until all answers are correct.# Create a [http://ssel-sched.eecs.umich.edu/sselScheduler/ResourceContact.aspx?tabindex=3&path=0:0:0:50020 Helpdesk Ticket{{#var:toolid}} helpdesk ticket] requesting trainingcheckout.# A Authorization will be provided pending demonstration of proper tool engineer will schedule a time for initial training.# Schedule a checkout session with use in the presence of a tool engineer via the helpdesk ticket system. If this checkout is successful, the engineer will authorize you on the tool.