==Checkout procedure==
<!-- Describe the checkout procedure # Complete a [[Lithography training session]]. If you have already completed this for the another tool, you do not need to complete it again. For example: --># Read through this page and the [https://docs.google.com/document/d/1cYUPWWE7AzkE-BRLHFfqDQG_HmtavqVICj8G6QGENdE/preview Standard Operating Procedure] User Manual above.
# Practice with your mentor or another authorized user until you are comfortable with tool operation.
# Complete Accurately complete the SOP quiz [https://docs.google.com/forms/d/e/1FAIpQLSfe7DBZ8Ldr8YxAGrgXpb-UVv8__o9ijhKKV5D6XxVyupvMcw/viewform?usp=sf_link here]. You may retake as necessary until all answers are correct.# Create a [http://ssel-sched.eecs.umich.edu/sselScheduler/ResourceContact.aspx?tabindex=3&path=0:0:0:{{#var:toolid}} Helpdesk Tickethelpdesk ticket] requesting trainingcheckout.# A Authorization will be provided pending demonstration of proper tool engineer will schedule a time for initial training.# Schedule a checkout session with use in the presence of a tool engineer via the helpdesk ticket system. If this checkout is successful, the engineer will authorize you on the tool.
==Maintenance==
The UV energy at the chuck face is routinely calibrated, so that the energy delivered corresponds to the display on the lamp controller. The energy delivered is 20 mJ/sec at the 405 nm wavelength with an additional 9-10 mJ/sec at the 365 nm wavelength (the 365 nm peak is not calibrated, but is constant in relation to the 405 nm peak). Lamp uniformity is routinely calibrated to within 2-3% across the 75 mm range.
The WEC (Wedge Error Compensation) head is completely rebuilt semi annually and checked weekly and adjusted as needed for proper height and level.