AZ 12XT

21 bytes added, 1 year ago
** 2-4K 3 minutes on a 110°C hotplate with the lid lowered
**1K 4 minutes on a 110°C hotplate with the lid lowered
*Exposure(see characterization data below)
**10-17um layers
***Contact Alingers 12-16 sec
***Stepper 0.22-0.24 sec, Focus -30 to -50
**>17um
***Contact Alingers 20-24sec