* HMDS in YES Image Reversal Oven
*Spin AZ 12xt
**When dispensing the AZ 12xt try to spread the puddle around as you dispense. You can get good even coverage with less resist this way.
**AZ 12xt is a high viscosity resist and will create stringers or cotton candy when spun.
**For 4 inch or larger samples you need to knock down the stringers with a swab or acetone between samples.
*Softbake
** 2-4K 3 minutes on a 110°C hotplate with the lid lowered