AZ 12XT

1 byte added, 10 months ago
no edit summary
Users should note that this is not a DNQ resist and is not compatible with the image reversal process used in the [[Image Reversal Oven|YES-310TA]].
*On 1/18/22 our contact aligner lamps are being re calibrated. This may reduce the required exposure by up to 22%. This page will be updated after we have time verify the new exposure times.
==Procedure==
===for 10-25um layers===