Lab 18-2 is a [[Sputter_deposition|sputter deposition ]] tool used for the application of very thin films; 10-2000nm. This tool is set up to deposit a range of metals primarily: Au, Ti, Pt, Cr, W, Al and Ir. Most deposited films are precise to +/-1 nm.