Difference between revisions of "ACS 200 cluster tool"

From LNF Wiki
Jump to navigation Jump to search
Line 57: Line 57:
 
<!-- We recommend creating a subpage detailing the supported processes for the tool, which will be generated if you leave the link below. Alternatively, you may include the information on this page. In that case, the Supported Processes document from the equipment manual can be included here, using {{#widget:GoogleDoc|key=googledocid}} -->
 
<!-- We recommend creating a subpage detailing the supported processes for the tool, which will be generated if you leave the link below. Alternatively, you may include the information on this page. In that case, the Supported Processes document from the equipment manual can be included here, using {{#widget:GoogleDoc|key=googledocid}} -->
  
There are several processes for this tool supported by the LNF, which are described in more detail on the [[/Processes/]] page.
+
There are several processes for this tool supported by the LNF, which are described in more detail on the [[/SPR 220/]] and [[/SPR 955/]] page.
  
 
<!-- If you allow custom recipes, let users know to contact a tool engineer, and you may also create the link below which will create a page that users can add custom recipes to. -->
 
<!-- If you allow custom recipes, let users know to contact a tool engineer, and you may also create the link below which will create a page that users can add custom recipes to. -->

Revision as of 10:16, 6 February 2019

ACS 200 cluster tool
54040.jpg
Equipment Details
Technology Lithography
Materials Restriction Semi-Clean
Material Processed SPR 220, SPR 955 0.9, and LNF approved photo resist syringes
Chemicals Used MF 300, MF 319, EBR, Acetone, HMDS
Equipment Manual
Overview System Overview
Operating Procedure SOP
Supported Processes Supported Processes
User Processes User Processes
Maintenance Maintenance



The ACS 200 cluster tool is an automated photoresist coating, baking, vapor prime, stripping and developing tool. It can run full 4" and 6" cassettes of up to 25 wafers at a time. It's capable of having multiple paths running simultaneously (ie., coating and developing from two different cassettes). It automatically pumps SPR 220-(3.0) and 955 photoresists. Other resists can be set up to automatically dispense from a syringe. The spinner's closed lid option can help aid with more uniform sidewall coating. HMDS is applied via vapor prime. Both developers are CMOS compatible (MF 319, and MF 300). The developer temperature is controlled to within 0.1°C throughout the process.

Announcements

  • Currently the developer module is down on the ACS. The parts have been back ordered and are suppose to arrive at latest Thursday February 14th. Please create a ticket if you have a time sensitive project.

Capabilities

  • Automated spin coating
  • Automated spray developing
  • Automated vapor prime
  • Photoresist stripping
  • 4" and 6" wafers
PMMA and other e-beam resists should be processed in Photoresist Bench 31 in 1480A
Any other non standard photoresist must have direct approval of tool owner
SU-8 may only be processed in the ROBIN lab

System overview

Hardware details

  • RC-8 spin coater with gyrset closed cover option
  • Spinner equipped with back side rinse arm for 4" wafers only
  • 4" chuck will accommodate 6"
  • SPR 220-(3.0) and SPR 955 0.9 photo resists automatically dispensed.
  • All other approved resists can be coated with EFD dispense option.
  • Spray develop module fitted with MF 300 and MF 319
  • Hot plate ovens and HMDS vapor prime chamber
  • Fully automated robot handling

Substrate requirements

  • 4" and 6" wafers
  • Glass wafers not preferred for baking

Material restrictions

The ACS 200 cluster tool is designated as a Semi-Clean class tool. Below is a list of approved materials for the tool. Approved means the material is allowed in the tool under normal circumstances. If a material is not listed, please create a helpdesk ticket or email info@lnf.umich.edu for any material requests or questions.


Supported processes

There are several processes for this tool supported by the LNF, which are described in more detail on the SPR 220 and SPR 955 page.

In addition to these, users can create a helpdesk ticket requesting a modification of one of the standard recipes by a tool engnineer. Some of these recipes are documented on ACS 200 cluster tool user processes.

Standard operating procedure

Widget text will go here.

Checkout procedure

  1. Read through this page and the Standard Operating Procedure above.
  2. Practice with your mentor or another authorized user until you are comfortable with tool operation.
  3. Complete the SOP quiz here
  4. Create a Helpdesk Ticket requesting training/checkout.
  5. A tool engineer will schedule a time for training/checkout

Maintenance

Complete spinner clean and conditioning are done semi annually or as needed. Fluid and resist fills are done/checked weekly. Hot plate ovens checked bi weekly and cleaned as needed. Spray develop checked weekly and maintained as needed. Robot training performed annually or as needed.