Acid Bench 12
This article does not follow the Equipment boilerplate. The article should be reorganized to comply with The LNF wiki's quality standards. |
This wet bench is used for working with acids, mostly for etching metals, pattering and cleaning substrates that have had metals on them. It is considered a metals bench, so wafers with metal are allowed in the bench with some restrictions. It is intended for use with 4” and 6” Si and glass substrates only. Only the processes listed below are allowed in this bench.
Acid Bench 12 | |
---|---|
Acid Bench 12 | |
Equipment Details | |
Technology | Wet bench |
Materials Restriction | Metals |
Material Processed | Silicon and Glass wafers |
Sample Size | 4" and 6" |
Chemicals Used | |
Equipment Manual | |
Overview | System Overview |
Operating Procedure | SOP |
Supported Processes | Processes |
Maintenance | Maintenance |
This page has not been released yet. |
Contents
Announcements
- Update this with announcements as necessary
System Overview
Chemicals Allowed
- Aluminum Etch
- Buffered HF (BHF)
- Hydrofluoric acid (HF)
- Chromium Etch
- Hydrochloric acid (HCl)
- Hydrogen peroxide (H2O2)
- Gold Etch
- Nanostrip
- Nitric acid (HNO3)
- Sulfuric acid (H2SO4)
Hardware Details
This bench contains 2 heated chemical baths, DI quick dump rinse tank (QDR), timers, and 4 unheated chemical baths.
Safety
Warning: | You must use the buddy system for all chemical processing. No processing if you are alone in the lab. If the yellow warning lights are on it means that there are 2 or 1 people in the lab. |
Working with chemicals can be very dangerous. Chemicals used at this bench are some of the most hazardous in the lab. To minimize the chance of accident, make sure you always:
- Wear personal protective equipment. Required PPE at this bench is an apron, face shield, and Trionic gloves.
- Know the properties and hazards of chemicals you are working with. If you don’t know, find out by reading about them or asking staff.
- Plan the details of your process. Before you start working, plan what quantities of chemicals and sample carriers you will use. Plan how you will rinse your sample and what you will do with any waste generated. Make sure you know how the controllers work.
- Only process 4” and 6” wafers.
- Do not use this bench without proper training.
- Waste from this bench goes into the LNF’s acid waste neutralization system and then to city sewers.
- No solvents can be used or disposed of here.
- Solutions which contains toxic materials that cannot be removed by neutralization (such as gold and chromium etch) should not be aspirated or disposed of down the drain.
Substrate Requirements
- 4 and 6 inch wafers
- Glass and Silicon
Material Restrictions
The Acid Bench 12 is designated as a Metals class tool. Below is a list of approved materials for the tool. Approved means the material is allowed in the tool under normal circumstances. If a material is not listed, please create a helpdesk ticket or email info@lnf.umich.edu for any material requests or questions.
Supported Processes
This section requires expansion. |
LNF Standard Processes in this bench
Widget text will go here.
Standard Operating Procedure
Widget text will go here.
Checkout Procedure
- Take the General Wet Bench Training, if you haven't already.
- Read through this page and the Standard Operating Procedure above.
- Practice with your mentor or another authorized user until you are comfortable with tool operation.
- Open a helpdesk ticket and request a checkout.
- A tool engineer will schedule a time for checkout.
- Complete the Acid Bench 12 quiz.
- If you pass the quiz the tool engineer will authorize you on the tool. If not you will be contacted to repeat.
Maintenance
- Bench is checked for issues twice a week during lab clean
- Nanostrip is changed weekly
- Chrome etch and gold etch are changed monthly
User supported maintenance
Please only make the following changes if you have been trained and are comfortable doing this. If you have an issue that is not detailed or are not trained please create a helpdesk ticket.