Acid Bench 12/Processes/Chromium Etch

From LNF Wiki
< Acid Bench 12‎ | ProcessesRedirect page
Jump to navigation Jump to search

Redirect to:

Warning Warning: This page has not been released yet.
About this Process
Process Details
Equipment Acid Bench 12
Technology Process
Material Cr
Chemicals Used Chromium Etch



This process describes the use of Chromium Etch in Acid Bench 12 for wet etching Chrome.

Procedure

Widget text will go here.

Characterization

Etch/Dep Rate

750 Ang/min

Uniformity

Mask Selectivity

Limitations

Qualification