This process describes the use of Chromium Etch in Acid Bench 12 for wet etching Chrome.
About this Process | |
---|---|
Process Details | |
Equipment | Acid Bench 12 |
Technology | Process |
Material | Cr |
Chemicals Used | Chromium Etch |
Contents
Procedure
Widget text will go here.
Characterization
Etch/Dep Rate
750 Ang/min