This page lists the processes supported by the LNF for the [[{{BASEPAGENAME}}]].
 
This page lists the processes supported by the LNF for the [[{{BASEPAGENAME}}]].
HF/Nitric Si etch
+
* HF/Nitric Si etch
Copper Pulse Plating
+
* Copper Pulse Plating
Nickel Pulse Plating
+
* Nickel Pulse Plating
Indium Plating
+
* Indium Plating
Piranha Clean
+
* Piranha Clean
RCA Clean
+
* RCA Clean
Gold  Etch
+
* Gold  Etch
Nickel Etch
+
* Nickel Etch
Copper Etch
+
* Copper Etch
  
 
<!-- Include google doc for supported processes document here -->
 
<!-- Include google doc for supported processes document here -->

Revision as of 13:13, 18 November 2016

Warning Warning: This page has not been released yet.

Description

This page lists the processes supported by the LNF for the Acid Bench 92.

  • HF/Nitric Si etch
  • Copper Pulse Plating
  • Nickel Pulse Plating
  • Indium Plating
  • Piranha Clean
  • RCA Clean
  • Gold Etch
  • Nickel Etch
  • Copper Etch