Aluminum is a metal that is a silvery-white, soft, non-magnetic and ductile in the boron group.
Contents
Applications
- Discuss common uses/applications for this material. Why this materials is used in the LNF?
Processing Equipment
Process technologies that can be used to deposit/pattern this material. If this is a substrate, refer to what tool/process restrictions there may be and possibly remove the following sub-sections.
Deposition Equipment
Etching Equipment
- Acid Bench 12 - maintained tank
- Acid Bench 73 - Beaker
- Acid Bench 80 - Beaker
- LAM 9400
Depositoin Processes
Etch Processes
- Wet etching
- Wet etching can be used to etch aluminum using Aluminum Etch at 50°C at Acid Bench 12, Acid Bench 73, and Acid Bench 80
- Reactive ion etching
References
- Etch rates for micromachining processing https://ieeexplore.ieee.org/abstract/document/546406
- Etch rates for micromachining processing-Part II https://ieeexplore.ieee.org/abstract/document/1257354