Chromium is a steely-grey, lustrous, hard, and brittle transition metal.
Contents
Processing Equipment
Deposition Equipment
Etching Equipment
Wet Etching
RIE
Applications
Common uses of Chromium include:
- masks
Processes
Deposition
Etching
Wet Etching
Wet etching is done using Transene Chromium Etch. Chromium Etch is a mixture of ceric ammonium nitrate, nitric acid, and water.