Chromium is a steely-grey, lustrous, hard, and brittle transition metal.

Processing Equipment

Deposition Equipment

Etching Equipment

Wet Etching

RIE

Applications

Common uses of Chromium include:

  • masks

Processes

Deposition

Etching

Wet Etching

Wet etching is done using Transene Chromium Etch. Chromium Etch is a mixture of ceric ammonium nitrate, nitric acid, and water.