Difference between revisions of "Deep UV SenLights PL16"

From LNF Wiki
Jump to navigation Jump to search
Line 5: Line 5:
 
|size = pieces up to a 6" wafer
 
|size = pieces up to a 6" wafer
 
|gases = [[ozone]]
 
|gases = [[ozone]]
|overview = [??? System Overview]
+
|sop = [https://drive.google.com/file/d/1gmxOsaavqGzBQ6lXpMfRsU0fSW7fTVpo/view?usp=sharing SOP]
|sop = [??? SOP]
 
 
|processes = [??? Supported Processes]
 
|processes = [??? Supported Processes]
 
|manufacturer = [http://www.senlights.com/ SenLights]
 
|manufacturer = [http://www.senlights.com/ SenLights]
Line 39: Line 38:
  
  
==Standard operating procedure==
+
==Equipment Manual==
{{#widget:GoogleDoc|key=???}}
+
[https://drive.google.com/file/d/1gmxOsaavqGzBQ6lXpMfRsU0fSW7fTVpo/view?usp=sharing Equipment Manual]
  
 
==Checkout procedure==
 
==Checkout procedure==
# Read through this page and the Standard Operating Procedure above.
+
# Read through this page and the [https://drive.google.com/file/d/1gmxOsaavqGzBQ6lXpMfRsU0fSW7fTVpo/view?usp=sharing Equipment Manual]
 
# Complete the SOP quiz
 
# Complete the SOP quiz
 
# Create a [http://ssel-sched.eecs.umich.edu/sselScheduler/ResourceContact.aspx?tabindex=3&path=0:0:0:{{#var:toolid}} Helpdesk Ticket] requesting checkout.
 
# Create a [http://ssel-sched.eecs.umich.edu/sselScheduler/ResourceContact.aspx?tabindex=3&path=0:0:0:{{#var:toolid}} Helpdesk Ticket] requesting checkout.

Revision as of 12:24, 14 October 2019

Deep UV SenLights PL16
59000.jpg
Equipment Details
Manufacturer SenLights
Model PL16
Technology Lithography
Materials Restriction Metals
Material Processed Photoresist
Sample Size pieces up to a 6" wafer
Gases Used ozone
Equipment Manual
Operating Procedure SOP
Supported Processes [??? Supported Processes]


Warning Warning: This page is under construction (Oct 2019)


The SenLights PL16 is a Deep UV exposure tool that can be used for ozone cleaning, hard-baking photoresist, and surface treatments.


Capabilities

  • Surface cleaning via ozone
  • Polymer etching va ozone
  • Positive photoresist (novolac based) crosslinking
  • PDMS Surface Modification
  • Surface prep for low temp fusion bonding

System overview

Hardware details

  • Aprox. 15 mW/cm2 at 30mm of 254nm light
  • 185nm light for ozone generation
  • Low concentrations of ozone in the range of 20-200ppm

Substrate requirements

  • Pieces to a 150mm wafer, up to 70mm thick

Material restrictions

The Deep UV SenLights PL16 is designated as a Metals class tool. Below is a list of approved materials for the tool. Approved means the material is allowed in the tool under normal circumstances. If a material is not listed, please create a helpdesk ticket or email info@lnf.umich.edu for any material requests or questions.



Equipment Manual

Equipment Manual

Checkout procedure

  1. Read through this page and the Equipment Manual
  2. Complete the SOP quiz
  3. Create a Helpdesk Ticket requesting checkout.


Qualification

The etch rate of a 100mm Si wafer coated with SPR 955 is monitored on a aprox. biweekly basis.