Difference between revisions of "Deposition"

From LNF Wiki
Jump to navigation Jump to search
Line 11: Line 11:
  
 
===Electrodeposition/ Electroplating/ Electrochemical deposition (ECD)===
 
===Electrodeposition/ Electroplating/ Electrochemical deposition (ECD)===
[https://en.wikipedia.org/wiki/Electroplating Electrodeposition]  
+
[https://en.wikipedia.org/wiki/Electroplating Electrodeposition]
 +
Electrodeposition, Which is available at LNF for Au, Cu, Ni, In, Ag, NiFe and ZnO; is the technique recommended when metal layers of more than a micron of thickness are needed.  The principle is simple: positive ions are attracted to the negative electrode (anode which is the sample in the case of metal deposition) and negative ions travel towards the cathode or positive electrode.  an electrochemical cell, which consists of a cathode, anode and electrolyte that contains the ion to be deposited is the main.
  
 
===Physical vapor deposition (PVD)===
 
===Physical vapor deposition (PVD)===

Revision as of 16:06, 14 January 2016

Deposition is any process that grows, coats, or otherwise transfers a material onto the substrate.

Technologies

Typical technologies include atomic layer deposition (ALD), chemical vapor deposition (CVD), electrodeposition/ electroplating or electrochemical deposition (ECD), and physical vapor deposition (PVD).

Atomic layer deposition (ALD)

Atomic Layer Deposition (ALD) at the LNF is performed on the Oxford OpAL ALD system that currently offers three films Alumina/Aluminum Oxide (Al2O3), Hafnia/Hafnium Oxide (HfO2), and Zinc Oxide (ZnO).

Chemical vapor deposition (CVD)

Chemical vapor deposition (CVD) consists of the substrate being exposed to one or more volatile precursors, which react and/or decompose on the substrate surface to produce the desired deposit. There are many methods for enhancing the chemical reaction rates of the precursors. The LNF has fourteen Low Pressure CVD (LPCVD) furnace tubes and five Plasma Enhanced CVD (PECVD) chambers.

Electrodeposition/ Electroplating/ Electrochemical deposition (ECD)

Electrodeposition Electrodeposition, Which is available at LNF for Au, Cu, Ni, In, Ag, NiFe and ZnO; is the technique recommended when metal layers of more than a micron of thickness are needed. The principle is simple: positive ions are attracted to the negative electrode (anode which is the sample in the case of metal deposition) and negative ions travel towards the cathode or positive electrode. an electrochemical cell, which consists of a cathode, anode and electrolyte that contains the ion to be deposited is the main.

Physical vapor deposition (PVD)

Physical vapor deposition (PVD) describes a variety of vacuum deposition methods used to deposit thin films by the condensation of a vaporized form of the desired film material onto various substrates.

Figures of merit

Deposition rate

The amount of material deposited in units of time, typically expressed in angstroms per second or minute.

Refractive index

Defines optical properties of a given material for a specific frequency or wavelength of light. Also known as index of refraction n.

Film Stress

The elastic mismatch between the thin film deposited and the substrate that results in a change in substrate curvature. Residual stress is typically defined by a unit of measurement (MPa) across a given area.

Thermal budget

Segregation