Difference between revisions of "EVG 510"

From LNF Wiki
Jump to navigation Jump to search
Line 55: Line 55:
 
<!-- We recommend creating a subpage detailing the supported processes for the tool, which will be generated if you leave the link below. Alternatively, you may include the information on this page. In that case, the Supported Processes document from the equipment manual can be included here, using {{#widget:GoogleDoc|key=googledocid}} -->
 
<!-- We recommend creating a subpage detailing the supported processes for the tool, which will be generated if you leave the link below. Alternatively, you may include the information on this page. In that case, the Supported Processes document from the equipment manual can be included here, using {{#widget:GoogleDoc|key=googledocid}} -->
  
The supported processes for this tool are described in detail in the [https://docs.google.com/document/d/1GsFpinRQwpc62QqcHwTsUzP54pmih9ORinBD4AUMSS0/preview supported processes] page.  For a specific process the maximum chuck force should not exceed the guidelines below.
+
The supported processes for this tool are described in detail in the [https://docs.google.com/document/d/1GsFpinRQwpc62QqcHwTsUzP54pmih9ORinBD4AUMSS0/preview supported processes] document.  For a specific process the maximum chuck force should not exceed the guidelines below.
 
 
  
 
{| class="wikitable" style="text-align: center;"
 
{| class="wikitable" style="text-align: center;"

Revision as of 14:07, 18 August 2015


EVG 510
140031.jpg
Equipment Details
Technology Wafer bonding
Materials Restriction Metals
Material Processed Si, Glass
Sample Size pieces, 100 mm, 150 mm
Equipment Manual
Overview System Overview
Operating Procedure SOP
Supported Processes Processes
Maintenance Maintenance


The EVG 510 is a wafer bonder capable of bonding pieces up to 150 mm wafers. It is primarily used for polymer bonding and wafer mounting with WaferBOND, but can also be used for other other types of bonding. Generally the EVG 520IS should be used for non-polymer bonding since the chamber is less contaminated with as the chamber does not allow polymers making the tool cleaner. Also the CL200 Megasonic Cleaner can be used before bonding to reduce particulate.

Announcements

  • None at this time

Capabilities

  • Bonding
    • Polymer
    • Anodic
    • Eutectic
  • Wafer mounting via WaferBOND

System Overview

Hardware Details

  • Force
    • 0 to 10 kN
  • Vacuum
    • 1e-5 mBar
    • ACP 28G Backing pump with Turbo
  • Temperature
    • 20°C to 550°C
    • 45°C/min heating rate
    • Passive cooling (1°C/min)
  • Voltage
    • ± 2000 V
    • Up to 50 mA

Substrate Requirements

  • Pieces, 100 mm, 150 mm

Material Restrictions

The EVG 510 is designated as a Metals class tool. Below is a list of approved materials for the tool. Approved means the material is allowed in the tool under normal circumstances. If a material is not listed, please create a helpdesk ticket or email info@lnf.umich.edu for any material requests or questions.


Supported Processes

The supported processes for this tool are described in detail in the supported processes document. For a specific process the maximum chuck force should not exceed the guidelines below.

Chuck

Material

Force (kN)
150 mm 100 mm 75 mm 50 mm
Steady

State

While

Heating

Steady

State

While

Heating

Steady

State

While

Heating

Steady

State

While

Heating

Ti 60 8 30 4 1.5 1.5 6 1
Quartz 10 5 5 2 3 1 2 0.5

Standard Operating Procedure

Widget text will go here.

Checkout Procedure

  1. Read through this page and the Standard Operating Procedure above.
  2. Create a Helpdesk Ticket requesting training.
  3. A tool engineer will schedule a time for initial training.
  4. Practice with your mentor or another authorized user until you are comfortable with tool operation.
  5. Complete the SOP quiz here.
  6. Schedule a checkout session with a tool engineer via the helpdesk ticket system. If this checkout is successful, the engineer will authorize you on the tool.

Maintenance

Once a week the chucks are cleaned and inspected for damage. A monitor run is performed every other month on a 150 mm wafer to ensure that the tool is in good operating condition.