Difference between revisions of "Ellipsometry"
Jump to navigation
Jump to search
Line 18: | Line 18: | ||
==Method of operation== | ==Method of operation== | ||
− | |||
*Elliptically polarized light is reflected from the measurement sample and is analyzed in p- and s- vector components. | *Elliptically polarized light is reflected from the measurement sample and is analyzed in p- and s- vector components. | ||
**p- polarized light is in the plane of incidence | **p- polarized light is in the plane of incidence | ||
Line 34: | Line 33: | ||
− | *Since ellipsometry measures both intensity and phase information, thickness and optical constants can be extracted. [[Spectroscopic reflectometry]] only measures reflected intensity vs. wavelength and is only capable of extracting film thickness by using a fixed set of optical constants for the thin film material in a material file stored on the tool. | + | *Since ellipsometry measures both intensity and phase information, thickness and optical constants can be extracted. [[Spectroscopic reflectometry]] only measures reflected intensity vs. wavelength and is only capable of extracting film thickness by using a fixed set of optical constants for the thin film material in a material file stored on the tool. |
==Applications== | ==Applications== |
Revision as of 09:13, 10 October 2018
Ellipsometry | |
---|---|
Technology Details | |
Technology | Metrology |
Equipment | Woollam M-2000 Ellipsometer |
Ellipsometry uses elliptically polarized light reflected off of the measurement sample to allow for extraction of both thickness and optical constants (n,k or e1,e2) for transparent and semi-transparent thin films.
Contents
Method of operation
- Elliptically polarized light is reflected from the measurement sample and is analyzed in p- and s- vector components.
- p- polarized light is in the plane of incidence
- s- polarized light is perpendicular to that plane.
- Reflected p- and s- light will have different amplitude and phase shifts which depend on optical properties of the substrate and thin film and the film thickness. This causes polarization of the light to change.
- The change in polarization is measured as Delta (∆) and Psi (Ψ).
- Delta is the phase shift between the two vector components of the elliptically polarized light.
- Tan(Psi) is the amplitude attenuation ratio of the two components.
- A model is fit to this data to extract thin film thickness and optical parameters.
- Spectroscopic ellipsometry measures delta and psi vs. wavelength of light reflected off of the sample. Our Woollam M-2000 Ellipsometer is a spectroscopic tool. Ellipsometry measurement at only a single wavelength has shortcomings of a non-unique thickness solution (a thickness repetition cycle) and poor accuracy within a repeating cycle of certain film thickness ranges.

Delta and psi data vs. wavelength at multiple angles of incidence
- Since ellipsometry measures both intensity and phase information, thickness and optical constants can be extracted. Spectroscopic reflectometry only measures reflected intensity vs. wavelength and is only capable of extracting film thickness by using a fixed set of optical constants for the thin film material in a material file stored on the tool.
Applications
This section requires expansion. |
Ellipsometry is most often used for the characterization of thin film thickness and material optical constants.
Equipment
Woollam M-2000 Ellipsometer
Main article: Woollam M-2000 Ellipsometer
Spectroscopic ellipsometer with 190-1700nm wavelength range.
See also
References