(Stepper exposure matrix 350nm isolated trenches in 0.97µm of SPR 955. Substrate is Si, 5nm SiO2, 34nm Si3N4, 5nm SiO2 and should have ~10% reflection at 365nm (couldn't measure this directly). 100C 90 sec softbake 110C 90 sec PEB AZ 300 25sec ACS develop)
 
(Wrightsh uploaded a new version of File:350nm trenches low reflection.jpg)
 
(No difference)

Latest revision as of 12:07, 12 September 2019

Stepper exposure matrix 350nm isolated trenches in 0.97µm of SPR 955. Substrate is Si, 5nm SiO2, 34nm Si3N4, 5nm SiO2 and should have ~10% reflection at 365nm (couldn't measure this directly). 100C 90 sec softbake 110C 90 sec PEB AZ 300 25sec ACS develop

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current12:07, 12 September 2019Thumbnail for version as of 12:07, 12 September 20194,252 × 852 (389 KB)Wrightsh (talk | contribs)Stepper exposure matrix 350nm isolated trenches in 0.97µm of SPR 955. Substrate is Si, 5nm SiO2, 34nm Si3N4, 5nm SiO2 and should have ~10% reflection at 365nm (couldn't measure this directly). 100C 90 sec softbake, 110C 90 sec PEB, AZ 300 25sec ACS de...
  • You cannot overwrite this file.

The following page uses this file:

Metadata