File:500nm lines low reflection.jpg

From LNF Wiki
Revision as of 20:13, 11 September 2019 by Wrightsh (talk | contribs) (Stepper exposure matrix 500nm isolated lines in 0.97µm of SPR 955. Substrate is Si, 5nm SiO2, 34nm Si3N4, 5nm SiO2 and should have ~10% reflection at 365nm (couldn't measure this directly). 100C 90 sec softbake 110C 90 sec PEB AZ 300 25sec ACS develop)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to navigation Jump to search

Original file(8,504 × 852 pixels, file size: 491 KB, MIME type: image/jpeg)

Stepper exposure matrix 500nm isolated lines in 0.97µm of SPR 955. Substrate is Si, 5nm SiO2, 34nm Si3N4, 5nm SiO2 and should have ~10% reflection at 365nm (couldn't measure this directly).

100C 90 sec softbake 110C 90 sec PEB AZ 300 25sec ACS develop

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current12:00, 12 September 2019Thumbnail for version as of 12:00, 12 September 20198,504 × 852 (491 KB)Wrightsh (talk | contribs)Stepper exposure matrix 500nm isolated lines in 0.97µm of SPR 955. Substrate is Si, 5nm SiO2, 34nm Si3N4, 5nm SiO2 and should have ~10% reflection at 365nm (couldn't measure this directly). 100C 90 sec softbake, 110C 90 sec PEB, AZ 300 25sec ACS deve...
  • You cannot overwrite this file.

The following page uses this file:

Metadata