File:BHF SiO2 Etch Undercut SPR 955 DUV.jpg

From LNF Wiki
Revision as of 17:47, 6 December 2019 by Wrightsh (talk | contribs) (15min BHF etch of SiO2 with SPR 955 mask, 5min in DUV tool)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to navigation Jump to search

Original file(1,516 × 728 pixels, file size: 165 KB, MIME type: image/jpeg)

Summary

15min BHF etch of SiO2 with SPR 955 mask, 5min in DUV tool

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current17:47, 6 December 2019Thumbnail for version as of 17:47, 6 December 20191,516 × 728 (165 KB)Wrightsh (talk | contribs)15min BHF etch of SiO2 with SPR 955 mask, 5min in DUV tool