Original file(1,280 × 960 pixels, file size: 174 KB, MIME type: image/jpeg)

Etch profile using the LNF Oxynitride LF recipe on the STS Pegasus 4.

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current15:03, 16 May 2016Thumbnail for version as of 15:03, 16 May 20161,280 × 960 (174 KB)Kjvowen (talk | contribs)Etch profile using the LNF Oxynitride LF recipe on the STS Pegasus 4.