Original file(1,594 × 948 pixels, file size: 156 KB, MIME type: image/png)

SPR 955 on Si, exposed in stepper, developed in ACS. softbake: 100C 90 sec , PEB; 110C 90sec

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current12:27, 2 May 2018Thumbnail for version as of 12:27, 2 May 20181,594 × 948 (156 KB)Wrightsh (talk | contribs)
12:21, 2 May 2018Thumbnail for version as of 12:21, 2 May 20181,182 × 720 (109 KB)Wrightsh (talk | contribs)