Revision as of 11:03, 4 December 2019 by Wrightsh (talk | contribs) (SPR 955 patterned, then 5 min DUV exposure, 180C 30 min bake, then a second layer of SPR 955 patterned on top.)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to navigation Jump to search

Original file(1,280 × 960 pixels, file size: 155 KB, MIME type: image/jpeg)

Summary

SPR 955 patterned, then 5 min DUV exposure, 180C 30 min bake, then a second layer of SPR 955 patterned on top.