Summary

Isolated trench etched using LNF_Switched_poly in the STS Pegasus 4 for 1 min.

Licensing

I, the copyright holder of this work, hereby publish it under the following license:

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current15:03, 1 March 2021Thumbnail for version as of 15:03, 1 March 20211,280 × 960 (118 KB)Kjvowen (talk | contribs)Isolated trench etched using LNF_Switched_poly in the STS Pegasus 4 for 1 min.