GS-139 solid sources are designed for use in the temperature range 975-1075°C. Spreading resistance measurements of B diffusion depths at 1000C for varying diffusion times are shown below.
+
GS-139 solid sources are designed for creating shallow B junctions and should be used in the temperature range 975-1075°C. Spreading resistance measurements of B diffusion depths at 1000C for varying times are shown below.
  
 
[[File:GS139 Shallow Boron.png|none|500px|caption]]
 
[[File:GS139 Shallow Boron.png|none|500px|caption]]

Latest revision as of 15:25, 9 February 2017

GS-139 solid sources are designed for creating shallow B junctions and should be used in the temperature range 975-1075°C. Spreading resistance measurements of B diffusion depths at 1000C for varying times are shown below.

caption