Difference between revisions of "Lift-off"

From LNF Wiki
Jump to navigation Jump to search
Line 1: Line 1:
 
<!-- Make sure to categorize page as "Equipment" and its subcategory -->
 
<!-- Make sure to categorize page as "Equipment" and its subcategory -->
{{#ifeq: {{NAMESPACE}} | Template | | [[Category:Equipment]][[Category:Processes]]}}
 
 
{{warning|This page has not been released yet.}}
 
{{warning|This page has not been released yet.}}
  
Line 24: Line 23:
 
==References==
 
==References==
 
List any external references or attachments related to this technology.
 
List any external references or attachments related to this technology.
 +
 +
[[Category:Wet chemical processing]]

Revision as of 14:39, 9 November 2015

Warning Warning: This page has not been released yet.

The term liftoff refers to a method of metal patterning whereby the photoresist is patterned, the metal is deposited and the photoresist is removed from under the metal “lifting off” the metal where it is deposited on top of the resist. Some keys to effective liftoff processing are:

Method of operation

  • The metal must be much thinner than the thickness of the resist. For standard resist, > 5:1 is required.
  • For fine lines, LOR (lift off resist) is a good material for line definition. Contact a staff member for more information.
  • The metal must have good adhesion to the substrate.

Heating of the resist in solvent causes the resist to swell and break any connection to the patterns. Ultrasonic will break up the metal and remove any connections between the metal on the resist and the patterns remaining.

Materials

  • Evaporated materials liftoff better than sputtered
  • Sputtered materials require LOR or other special methods for liftoff
  • Not compatible with PECVD or other heated processes