<!-- We recommend creating a subpage detailing the supported processes for the tool, which will be generated if you leave the link below. Alternatively, you may include the information on this page. In that case, the Supported Processes document from the equipment manual can be included here, using {{#widget:GoogleDoc|key=googledocid}} -->
+
This tool is primarily used to expose photodefinable materials.  The lamp output is calibrated to the 405 nm peak at 20 mJ/sec with <5% uniformity across the 4” area. The 365 peak output is about half of this and tracks very well however is not routinely calibrated. We allow 4” masks, 5” masks, 7” masks, transparencies, shadow masking, or a manually timed flood exposure. 
  
This tool is primarily used to expose photodefinable materials.  The lamp output is calibrated to the 405 nm peak at 20 mJ/sec with 3% uniformity across the 4” area.  The 365 peak output is about half of this and tracks very well however is not routinely calibrated.  We allow 4” masks, 5” masks, 7” masks, transparencies, shadow masking, or a manually timed flood exposure. 
+
Exposure of all LNF approved photoresists are allowed on this tool, for data on specific resist please see that resists wiki page.
 
 
Exposure of all LNF approved photoresists are allowed on this tool in accordance with standard operating procedure.  More data on exposure times can be found on datasheet for the specific [[photoresist]].
 
 
 
<!-- If you allow custom recipes, let users know to contact a tool engineer, and you may also create the link below which will create a page that users can add custom recipes to. -->
 
In addition to these, this tool has a number of user-created recipes for etching a wide variety of materials. Some of these recipes are documented on [[LNF User:{{BASEPAGENAME}} User Processes|{{BASEPAGENAME}} user processes]]. If you are curious if your material can be processed in this tool, please contact the tool engineers via the helpdesk ticket system.
 
  
 
==Standard operating procedure==
 
==Standard operating procedure==

Revision as of 13:21, 3 November 2017

MA6 Mask Aligner
50101.jpg
Equipment Details
Technology Contact Lithography
Materials Restriction Semi-Clean
Material Processed Photoresist
Mask Materials 4", 5", 7" mask plates
Sample Size 4" and 6" wafers. Pieces with staff approval
Chemicals Used LNF approved photoresists
Equipment Manual
Overview System Overview
Operating Procedure SOP
Supported Processes Supported Processes
Maintenance Maintenance


The MA6 Mask Aligner is primarily used to expose photo-definable materials. We allow 4” masks, 5” masks, 7” masks, transparencies, shadow masking, or just flood exposure.

Capabilities

  • 2 µm min feature size resolution in thin resist
  • Aspect Ratio 1:3 fairly standard
  • Substrate thickness 200 µm to 4 mm possible

System overview

Hardware Details

  • Broadband light source calibrated to 20 mJ/sec at the 405 nm peak. Total broadband dose about 30 mJ/sec
  • 4" and 6" chucks
  • 4", 5" and 7" mask holders
  • Flood exposure, soft, hard, and vacuum contact capable
  • Topside alignment (no backside or bond alignment)
  • 10 mm stage travel, 150 mm microscope objective travel with split field view camera option

Substrate requirements

  • Full 4" and 6" wafers standard
  • Mounting may be necessary if wafer has thru holes, etc. Create helpdesk ticket for assistance
  • Substrate thickness 200 µm to 4 mm possible

Material restrictions

Allowed Materials - LNF approved photoresists

Not Allowed Materials - Uncured PDMS and SU-8 (restricted w/out approval)

Supported processes

This tool is primarily used to expose photodefinable materials. The lamp output is calibrated to the 405 nm peak at 20 mJ/sec with <5% uniformity across the 4” area. The 365 peak output is about half of this and tracks very well however is not routinely calibrated. We allow 4” masks, 5” masks, 7” masks, transparencies, shadow masking, or a manually timed flood exposure.

Exposure of all LNF approved photoresists are allowed on this tool, for data on specific resist please see that resists wiki page.

Standard operating procedure

Checkout procedure

  1. Read through this page and the Standard Operating Procedure above.
  2. Create a Helpdesk Ticket requesting training.
  3. A tool engineer will schedule a time for initial training.
  4. Practice with your mentor or another authorized user until you are comfortable with tool operation.
  5. Schedule a checkout session with a tool engineer via the helpdesk ticket system. If this checkout is successful, the engineer will authorize you on the tool.

Maintenance

The UV energy at the chuck face is routinely calibrated, so that the energy delivered corresponds to the display on the lamp controller. The energy delivered is 20 mJ/sec at the 405 nm wavelength with an additional 9-10 mJ/sec at the 365 nm wavelength (the 365 nm peak is not calibrated, but is constant in relation to the 405 nm peak). Lamp uniformity is routinely calibrated to within 2-3% across the 150 mm range. The WEC (Wedge Error Compensation) head is completely rebuilt semi annually and checked monthly and adjusted as needed for level.