The LNF uses a wide variety of processes and materials, some of which can cause contamination to others' processes.  In order to reduce the possibility of contamination, the lab places material restrictions on each tool.  There are three main levels of material restrictions in the LNF, described in detail below.  They are CMOS Clean, Semi-Clean, and Metals.  The materials listed in each section are an example of what may be allowed in a tool with that level. A complete list may be found on individual [[:Category:Equipment|tool]] pages.
+
The LNF uses a wide variety of processes and materials, some of which can cause contamination to others' processes.  In order to reduce the possibility of contamination, the lab places material restrictions on each tool.  There are four main levels of material restrictions in the LNF, described in detail below.  They are CMOS Clean, Semi-Clean, Metals, and General.  The materials listed in each section are an example of what may be allowed in a tool with that level. A complete list may be found on individual [[:Category:Equipment|tool]] pages.
  
 
==CMOS clean==
 
==CMOS clean==
 
CMOS clean tools are considered the lowest level of possible contamination and thus have the greatest level of restriction.  In order for one's sample to run in a CMOS Clean tool, it must have only have CMOS clean materials '''and''' only ever be processed in CMOS clean tools.  Some of these tools also require an additional clean, such as a [[Pre Furnace Clean]].  Please see individual tool pages for details.
 
CMOS clean tools are considered the lowest level of possible contamination and thus have the greatest level of restriction.  In order for one's sample to run in a CMOS Clean tool, it must have only have CMOS clean materials '''and''' only ever be processed in CMOS clean tools.  Some of these tools also require an additional clean, such as a [[Pre Furnace Clean]].  Please see individual tool pages for details.
  
===Material Restrictions===
 
 
Here is an example list of materials allowed in CMOS Clean tools.
 
Here is an example list of materials allowed in CMOS Clean tools.
 
Wafer used in CMOS Clean tools must be Prime Grade
 
Wafer used in CMOS Clean tools must be Prime Grade
Line 12: Line 11:
 
Semi-clean is the next level of material restrictions.  This level includes all materials in the CMOS Clean group as well as some low-mobility metals and films made in Semi-Clean tools.  CMOS Clean and Semi-Clean wafers may be processed in these tools. In order to go back to a CMOS Clean tool, additional cleans may be necessary.  For more information, see individual tool pages.
 
Semi-clean is the next level of material restrictions.  This level includes all materials in the CMOS Clean group as well as some low-mobility metals and films made in Semi-Clean tools.  CMOS Clean and Semi-Clean wafers may be processed in these tools. In order to go back to a CMOS Clean tool, additional cleans may be necessary.  For more information, see individual tool pages.
  
===Material Restrictions===
 
 
Here is an example list of materials allowed in Semi-Clean tools.
 
Here is an example list of materials allowed in Semi-Clean tools.
  
Line 20: Line 18:
 
Metals is the lowest level of segregation in the lab.  Most materials are allowed in these tools. Any sample processed in a Metals tool is not allowed back into a Semi-Clean or CMOS Clean tool without express permission from LNF staff, by creating a helpdesk ticket.  Additional cleans will be required.
 
Metals is the lowest level of segregation in the lab.  Most materials are allowed in these tools. Any sample processed in a Metals tool is not allowed back into a Semi-Clean or CMOS Clean tool without express permission from LNF staff, by creating a helpdesk ticket.  Additional cleans will be required.
  
===Material Restrictions===
 
 
Here is an example list of materials allowed in Metals tools.
 
Here is an example list of materials allowed in Metals tools.
  
Line 26: Line 23:
 
| title = Material list
 
| title = Material list
 
| content = {{#widget:ApprovedMaterials|toolid=3|header=N}}
 
| content = {{#widget:ApprovedMaterials|toolid=3|header=N}}
 +
}}
 +
 +
==General==
 +
General class tools allow most Metals class materials, however these systems have a low chance for cross-contamination and therefore the segregation class of a Semi-Clean or CMOS clean wafer is not altered by going through a general class system.  Most metrology and lithography equipment falls in this category.
 +
 +
Here is an example list of materials allowed in General tools.
 +
 +
{{Collapsible section
 +
| title = Material list
 +
| content = {{#widget:ApprovedMaterials|toolid=4|header=N}}
 
}}
 
}}

Revision as of 08:58, 25 October 2019

The LNF uses a wide variety of processes and materials, some of which can cause contamination to others' processes. In order to reduce the possibility of contamination, the lab places material restrictions on each tool. There are four main levels of material restrictions in the LNF, described in detail below. They are CMOS Clean, Semi-Clean, Metals, and General. The materials listed in each section are an example of what may be allowed in a tool with that level. A complete list may be found on individual tool pages.

CMOS clean

CMOS clean tools are considered the lowest level of possible contamination and thus have the greatest level of restriction. In order for one's sample to run in a CMOS Clean tool, it must have only have CMOS clean materials and only ever be processed in CMOS clean tools. Some of these tools also require an additional clean, such as a Pre Furnace Clean. Please see individual tool pages for details.

Here is an example list of materials allowed in CMOS Clean tools. Wafer used in CMOS Clean tools must be Prime Grade

Semi-clean

Semi-clean is the next level of material restrictions. This level includes all materials in the CMOS Clean group as well as some low-mobility metals and films made in Semi-Clean tools. CMOS Clean and Semi-Clean wafers may be processed in these tools. In order to go back to a CMOS Clean tool, additional cleans may be necessary. For more information, see individual tool pages.

Here is an example list of materials allowed in Semi-Clean tools.

Metals

Metals is the lowest level of segregation in the lab. Most materials are allowed in these tools. Any sample processed in a Metals tool is not allowed back into a Semi-Clean or CMOS Clean tool without express permission from LNF staff, by creating a helpdesk ticket. Additional cleans will be required.

Here is an example list of materials allowed in Metals tools.

General

General class tools allow most Metals class materials, however these systems have a low chance for cross-contamination and therefore the segregation class of a Semi-Clean or CMOS clean wafer is not altered by going through a general class system. Most metrology and lithography equipment falls in this category.

Here is an example list of materials allowed in General tools.