{{ safesubst:#invoke:Unsubst||$N=Merge |date=__DATE__ |$B= {{#invoke:Message box|mbox}} }} Microposit Developer Concentrate is developer produced by Shipley. It uses alkaline phosphate salts to develop the photoresist. It attacks aluminum slower then TMAH based developers, however it XYZ. It is used in the CEE Developer 2, mixed 50:50 with DI water.