Technology | Direct writing |
Materials Restriction | Metals |
Material Processed | no restrictions |
Mask Materials | na |
Sample Size | 50x50 mm 5 mm height |
Chemicals Used | na |
Gases Used | na |
Equipment Manual | |
Overview | System Overview |
Operating Procedure | SOP |
Supported Processes | Supported Processes |
User Processes | User Processes |
Maintenance | Maintenance |
The NanoInk DPN 5000 is a...
Contents
Announcements
- Update this with announcements as necessary
Capabilities
- Etch Rate
- Resolution
- Aspect Ratio
- Thickness range
System overview
Hardware details
- Gases
- Pressure
- Chuck
- Chamber
- RF / Power Specs
- Chemicals
Substrate requirements
- Wafer Size
- Wafer type
- Any mounting?
- Wafer thickness
Material restrictions
The NanoInk DPN 5000 is designated as a Metals class tool. Below is a list of approved materials for the tool. Approved means the material is allowed in the tool under normal circumstances. If a material is not listed, please create a helpdesk ticket or email info@lnf.umich.edu for any material requests or questions.
Supported processes
There are several processes for this tool supported by the LNF, which are described in more detail on the Processes page.
In addition to these, this tool has a number of user-created recipes for etching a wide variety of materials. Some of these recipes are documented on NanoInk DPN 5000 user processes. If you are curious if your material can be processed in this tool, please contact the tool engineers via the helpdesk ticket system.
Standard operating procedure
Widget text will go here.
Checkout procedure
- Read through this page and the Standard Operating Procedure above.
- Complete the training request form here.
- Create a Helpdesk Ticket requesting training.
- A tool engineer will schedule a time for initial training.
- Practice with your mentor or another authorized user until you are comfortable with tool operation.
- Complete the SOP quiz here.
- Schedule a checkout session with a tool engineer via the helpdesk ticket system. If this checkout is successful, the engineer will authorize you on the tool.
Maintenance
Process name