* Nickel can be etched with [[Piranha]] (380 nm/min), dilute [[Aqua regia]] (100 nm/min)
+
* Nickel can be etched with [[Piranha Etch]] (380 nm/min), dilute [[Aqua Regia]] (100 nm/min)
  
 
===Characterization Processes===
 
===Characterization Processes===

Revision as of 12:41, 20 April 2020

Warning Warning: This page has not been released yet.

Nickel (Ni) is an element with the atomic number 28. It is silvery-white and lustrous in appearance with a slightly golden tinge. Nickel is a transition metal and is a very hard and ductile material.

Equipment

Process technologies that can be used to deposit/pattern this material.

Deposition Equipment

Etching Equipment

Characterization Equipment

  • Metrology/Characterization equipment available in the LNF for measuring physical, optical, and surface properties of this material.

Applications

  • Discuss common uses/applications for this material. Why this materials is used in the LNF?

Processes

Deposition Processes

  • List of technologies for depositing this material and relevant process information specific to this material associated with this equipment/type of process.

Etching Processes

Characterization Processes

  • List of techniques for metrology/characterization can be used with this material and relevant process information specific to this material associated with this equipment/type of process.

Other Relevant Material Information

Technical Data

  • Charts or specific LNF related data for this material.