Lab 18-2 is a magnetron [[sputter deposition]] tool for depositing conductive metallic films. Sputter deposition is achieved by bombarding a source material with energetic ions, typically Ar+. Atoms at the surface of the target are knocked loose, and transported to the surface of the substrate, where deposition occurs. Electrically conductive material such as Al, W, and Ti can use a dc power source, in which the target acts as the cathode in a diode system. Sputtering of dielectrics such as silicon dioxide, or aluminum oxide requires an Rf power source to supply energy to the argon atoms. Sputter films are ideal for sidewall coverage in low thermal budget cases for contact and insulating layers over features.  
+
The PVD 75 Proline is a magnetron [[sputter deposition]] tool for depositing conductive metallic and non conductive dielectric films. Sputter deposition is achieved by bombarding a source material with energetic ions, typically Ar+. Atoms at the surface of the target are knocked loose, and transported to the surface of the substrate, where deposition occurs. Electrically conductive material such as Al, W, and Ti can use a dc power source, in which the target acts as the cathode in a diode system. Sputtering of dielectrics such as silicon dioxide, or aluminum oxide requires an Rf power source to supply energy to the argon atoms. Sputter films are ideal for sidewall coverage in low thermal budget cases for contact and insulating layers over features.  
  
 
==Announcements==
 
==Announcements==
 
<!-- *Update this with announcements as necessary -->
 
<!-- *Update this with announcements as necessary -->
*The target configuration has been moved to the Supported Process section below. Follow the link to Lab 18-2/Processes. On that page under the Target Calendar header is the link to the calendar.
+
*The target change process on this tool is a user supported process. That can be completed during the tool reservation when the chamber is vented to load samples.
  
 
==Capabilities==
 
==Capabilities==
 
* Computer controlled recipes  
 
* Computer controlled recipes  
* Load lock supported processing
+
* Non Load lock configuration
 
* limited film stress versatility with in film development.
 
* limited film stress versatility with in film development.
 
* Reactive Film capabilities (Ar, O<sub>2</sub>, and N<sub>2</sub>)
 
* Reactive Film capabilities (Ar, O<sub>2</sub>, and N<sub>2</sub>)
  
 
==System Overview==
 
==System Overview==
The Lab 18-2 has a 18" D-shaped chamber with a load lock chamber to quickly load and unload samples without breaking high vacuum in the process chamber. The tools five magnetron sputtering sources are set up to allow for RF, DC, and DC co-sputtering. There is an additional Rf power supply on the substrate platen to allow for in situ sample cleans, and bias voltage to manipulate the film characteristics. Sample heating up to 500C is achieved by using the tools quartz heater lamps.
+
The Lab 18-2 has a 14" square-shaped chamber high vacuum process chamber. The tools four Tourus Mag Kepper magnetron sputtering sources are set up to allow for RF, DC, Pulse DC and DC co-sputtering. There is an additional Rf power supply on the substrate platen to allow for in situ sample cleans, and bias voltage to manipulate the film characteristics. Sample heating up to 350°C is achieved by using the tools quartz heater lamps.
  
 
===Hardware Details===
 
===Hardware Details===

Revision as of 13:59, 16 May 2016

< Sputter deposition

PVD 75 Proline
61081.jpg
Equipment Details
Technology PVD
Materials Restriction Metals
Material Processed Al,Cr,Cu,Au,Ge,Ir,Ni,NiCr,Pt,Si,Ag,Ti
Sample Size 150mm x 4mm and smaller samples
Gases Used Ar, N2, O2
Equipment Manual


The PVD 75 Proline is a magnetron sputter deposition tool for depositing conductive metallic and non conductive dielectric films. Sputter deposition is achieved by bombarding a source material with energetic ions, typically Ar+. Atoms at the surface of the target are knocked loose, and transported to the surface of the substrate, where deposition occurs. Electrically conductive material such as Al, W, and Ti can use a dc power source, in which the target acts as the cathode in a diode system. Sputtering of dielectrics such as silicon dioxide, or aluminum oxide requires an Rf power source to supply energy to the argon atoms. Sputter films are ideal for sidewall coverage in low thermal budget cases for contact and insulating layers over features.

Announcements

  • The target change process on this tool is a user supported process. That can be completed during the tool reservation when the chamber is vented to load samples.

Capabilities

  • Computer controlled recipes
  • Non Load lock configuration
  • limited film stress versatility with in film development.
  • Reactive Film capabilities (Ar, O2, and N2)

System Overview

The Lab 18-2 has a 14" square-shaped chamber high vacuum process chamber. The tools four Tourus Mag Kepper magnetron sputtering sources are set up to allow for RF, DC, Pulse DC and DC co-sputtering. There is an additional Rf power supply on the substrate platen to allow for in situ sample cleans, and bias voltage to manipulate the film characteristics. Sample heating up to 350°C is achieved by using the tools quartz heater lamps.

Hardware Details

  • Cryo pumped chamber – upper 10-7 Torr base pressure
  • Chamber capacity: single wafer
  • Configured with port for future load lock
  • Sample heating – up to 350°C
    • Four 3” Sputtering Guns
    • 2 DC (one pulse DC source) and 2 RF power supply (one for sample bias)

Substrate Requirements

  • Sample sizes: pieces, up to 6” wafers.
  • Wafer holders available for 2", 3", 4", 6"; as well as clip fixtures for smaller pieces
    • Diameter 150 mm maximum
    • Substrates up to 4 mm Thick. With special fixture up to 8 mm.

Material Restrictions

The PVD 75 Proline is designated as a Metals class tool. Below is a list of approved materials for the tool. Approved means the material is allowed in the tool under normal circumstances. If a material is not listed, please create a helpdesk ticket or email info@lnf.umich.edu for any material requests or questions.


Supported Processes

Basic "User" access with the Lab 18's provide researchers the ability to load, transfer samples, and deposit standard characterized materials. For more details, see PVD 75 Proline/Processes.

In addition to these, this tool has a number of user-supported recipes for depositing a wide variety of materials. Some of these recipes are documented on User Processes. If you are curious if your material can be deposited in this tool, please contact the tool engineers via the helpdesk ticket system.

Process Name

Multiple staff characterized films are available. If two thicknesses are listed the first is for per run and the second thickness is for total material used per reservation.

Material Max thickness (Run/Reservation)
Aluminum (Al) 1 µm / NA
Alumina/Aluminum Oxide (Al2O3) 1000Å / NA
Chrome (Cr) 2000Å / NA
Copper (Cu) 1000Å / 5000Å
Gold (Au) 5000Å / NA
Iron (Ir) 1000Å / 5000Å
Nickel (Ni) 5000 Å / 1 µm
Platinum (Pt) 5000 Å / 1 µm
Silver (Ag) 5000 Å / 1 µm
Titanium (Ti) 2000 Å / 5000 Å
Tungsten (W) 3000 Å / 9000 Å
Tungsten/Titanium (W-Ti) 3000 Å / 8000 Å

Standard Operating Procedure

Widget text will go here.

Checkout Procedure

The Lab 18-2 is on the LNF Scheduler. LNF constituents may reserve time on the tool, and even request staff support for process development. For more details, see Lab 18 access and training.

  1. Read through the Standard Operating Procedure above.
  2. Create a helpdesk ticket requesting training.
  3. A tool engineer will schedule a time for initial training.
  4. Practice with your mentor or another authorized user until you are comfortable with tool operation.
  5. Schedule a checkout session with a tool engineer via the helpdesk ticket system. If this checkout is successful, the engineer will authorize you on the tool.


Maintenance

For more details, see PVD 75 Proline/Maintenance and qualification.