Parylene deposition
Parylene deposition is a method for depositing parylene, a thin, transparent polymer coating that is conformal, usually pinhole free, has high dielectric strength, high surface and volume resistivity, and resists moisture, acids, alkalis, petroleum products and solvents. Parylene is also “body safe” which means it can be used to protect medical devices and implantable electronics.
Parylene deposition | |
---|---|
Technology Details | |
Technology | CVD |
Equipment | List of Parylene deposition equipment |
This page has not been released yet. |
Contents
Announcements
There are no announcements at this time.
Equipment
SCS PDS 2035CR
Materials
- Parylene C only
Method of operation
This section requires expansion. |
A solid, granular raw material, called dimer, is heated under under vacuum and vaporized into a dimeric gas at 100-150C. The gas is then pyrolized to cleave the dimer to its monomeric form. In the room temperature, vacuum, deposition chamber, the monomer gas deposits on all surfaces as a thin, transparent polymer film. .
Applications
This section is in a list format that may be better presented using prose. |
Medical
- Implanted medical devices
- Stents
- Electrosurgical tools
- Cochlear and ocular implants
- Medical electronics
Electronics
- Printed circuit boards and assemblies
- Sensors
- LEDs
- MEMS
- Capacitors
- Wafers
Automotive
- Electronics & Sensors
- LEDs
- Emissions Sensors
Aerospace
- MEMS
- Sensors
- Circuit card assemblies
Other
- Hydrophobic coating
- Barrier layers
- Corrosion protection
- Micro-structure reinforcement
Operating Procedures
Checkout procedure
- Create a Help desk Ticket requesting training.
- A process engineer will schedule a time for initial training. After completing training the user can attempt a checkout session. It may be necessary for some users to participate in more than one training session, prior to attempting check out.
- Schedule a checkout session with a tool engineer via the Help desk Ticket system. If this checkout is successful, the engineer will authorize you on the tool.
Maintenance