Photoresist is a photoactive polymer suspended in a solvent used in [[Lithography]] processing.  We have positive novolak based resists for use with our mask aligners and stepper, negative epoxy based resists ..... and e-beam resists for use with the JOEL.
 +
 +
==Applications==
 +
===Etch===
 +
====RIE====
 +
A photoresist used in RIE needs to be thermally stable and resistant to the etch chemistry.
 +
* SPR 220 - 3µm of SPR 220 is the most common etch mask at the LNF.
 +
* SPR 955 - 0.97µm of SPR 955 allows a higher resolution then SPR 220 when a thinner mask is acceptable.
 +
* KMPR - KMPR is a negative epoxy based photoresist with a very good etch resistance, but is more difficult to pattern and remove.
 +
* ZEP - This is an e-beam photoresist that generally has much better etch resistance then PMMA
 +
* PMMA 950 - PMMA can be used as an RIE mask, but will generally etch several times faster then the SPR series.
 +
 +
====Wet Etch====
 +
* S1800 - XXX of 1813 is our standard wet etch mask due to XXX
 +
 +
===Deposition===
 +
====Lift Off====
 +
Liftoff needs a photoresist profile that prevents sidewall deposition from bridging the film.  Generally this is done by using a bi-layer stack and undercutting the bottom layer...
 +
* 1813 on LOR
 +
* PMMA 950 on PMMA 450
 +
====Plating====
 +
  
<!-- Insert the tool description here -->
 
 
Below you can find a list of public and private approved photoresists for the LNF.  If you would like to bring a new photoresist into the robin lab or clean room, then please create a help desk ticket or email info@lnf.umich.edu. All photoresists must be handled using the green polychloroprene gloves.  
 
Below you can find a list of public and private approved photoresists for the LNF.  If you would like to bring a new photoresist into the robin lab or clean room, then please create a help desk ticket or email info@lnf.umich.edu. All photoresists must be handled using the green polychloroprene gloves.  
 
==Announcements==
 
==Announcements==

Revision as of 08:54, 26 June 2018

Photoresist is a photoactive polymer suspended in a solvent used in Lithography processing. We have positive novolak based resists for use with our mask aligners and stepper, negative epoxy based resists ..... and e-beam resists for use with the JOEL.

Applications

Etch

RIE

A photoresist used in RIE needs to be thermally stable and resistant to the etch chemistry.

  • SPR 220 - 3µm of SPR 220 is the most common etch mask at the LNF.
  • SPR 955 - 0.97µm of SPR 955 allows a higher resolution then SPR 220 when a thinner mask is acceptable.
  • KMPR - KMPR is a negative epoxy based photoresist with a very good etch resistance, but is more difficult to pattern and remove.
  • ZEP - This is an e-beam photoresist that generally has much better etch resistance then PMMA
  • PMMA 950 - PMMA can be used as an RIE mask, but will generally etch several times faster then the SPR series.

Wet Etch

  • S1800 - XXX of 1813 is our standard wet etch mask due to XXX

Deposition

Lift Off

Liftoff needs a photoresist profile that prevents sidewall deposition from bridging the film. Generally this is done by using a bi-layer stack and undercutting the bottom layer...

  • 1813 on LOR
  • PMMA 950 on PMMA 450

Plating

Below you can find a list of public and private approved photoresists for the LNF. If you would like to bring a new photoresist into the robin lab or clean room, then please create a help desk ticket or email info@lnf.umich.edu. All photoresists must be handled using the green polychloroprene gloves.

Announcements

  • None at this time.

Photoresist Table

Photoresists
Photoresist LNF/Private Tool +/-/Reversible Stored Notes
950K PMMA 6% LNF E-Beam Spinner ? Photoresist cabinet 1440C; 1480 photoresist -
AZ5214-E (IR) Private Not using +, Reversible No longer stored -
AZ9260 Sold through store ? + ? Thick photoresist, high resolution
KMPR 1010 Private CEE 100CB Spinner - ? UV, E-beam, x-ray, contact aligner
KMPR 1025 Private CEE 100CB Spinner - ? UV, E-beam, or x-ray
LOR 10B Lift-Off Resist Private CEE 100CB Spinner - ? -
Omni Coat ? ? ? ? -
S1813 LNF CEE 100 and CEE 200 Spinners + Photoresist cabinet 1440C -
SC1827 LNF/discontinued CEE 100 and CEE 200 Spinners + Photoresist cabinet 1440C -
SPR 220-3.0 LNF ACS 200 Cluster Tool, CEE 100 and CEE 200 Spinners + Photoresist cabinet 1440C -
SPR 220-7.0 LNF/Private CEE 100 and CEE 200 Spinners + Photoresist cabinet 1440C LNF provides the photoresist for the CEE 200CB Spinner #1, but it must be purchased if you want to use it on the CEE 100CB Spinner
SPR 955-0.9 LNF ACS 200 Cluster Tool, CEE 100 and CEE 200 Spinners + Photoresist cabinet 1440C Thinner viscosity, higher resolution
SU-8 2010 ? ROBIN Lab - Epoxy photoresist for micromachining
SU-8 2005 ? ROBIN Lab - Epoxy photoresist for micromachining
SU-8 2050 ? ROBIN Lab - Epoxy photoresist for micromachining