Difference between revisions of "Photoresist"

From LNF Wiki
Jump to navigation Jump to search
Line 3: Line 3:
  
  
 +
==LNF Supported Photoresists==
 +
...table...
  
 
==Applications==
 
==Applications==
 
===Etch===
 
===Etch===
====RIE====
+
* RIE - Photoresist used in RIE needs to be thermally stable and resistant to the etch chemistry.
A photoresist used in RIE needs to be thermally stable and resistant to the etch chemistry.
+
* Wet Etch - A photoresists adhesion is very important as any adhesion failure greatly increases undercut.
* SPR 220 - 3µm of SPR 220 is the most common etch mask at the LNF.
 
* [[SPR 955]] - 0.97µm of SPR 955 allows a higher resolution then SPR 220 when a thinner mask is acceptable.
 
* KMPR - KMPR is a negative epoxy based photoresist with a very good etch resistance, but is more difficult to pattern and remove.
 
* ZEP - This is an e-beam photoresist that generally has much better etch resistance then PMMA
 
* PMMA 950 - PMMA can be used as an RIE mask, but will generally etch several times faster then the SPR series.
 
 
 
====Wet Etch====
 
A photoresists adhesion is very important as any adhesion failure greatly increases undercut.
 
* S1800 - XXX of 1813 is our standard wet etch mask due to XXX
 
  
 
===Deposition===
 
===Deposition===
====Lift Off====
+
* Liftoff -  Need a photoresist profile that prevents sidewall deposition.  Often this is done by using a bi-layer stack and undercutting the bottom layer.
Liftoff needs a photoresist profile that prevents sidewall deposition.  Often this is done by using a bi-layer stack and undercutting the bottom layer.
+
* Plating
* 1813 on LOR
+
* Molding
* PMMA 950 on PMMA 450
 
====Plating====
 
====Molding====
 
  
  
 
Below you can find a list of public and private approved photoresists for the LNF.  If you would like to bring a new photoresist into the robin lab or clean room, then please create a help desk ticket or email info@lnf.umich.edu. All photoresists must be handled using the green polychloroprene gloves.
 
Below you can find a list of public and private approved photoresists for the LNF.  If you would like to bring a new photoresist into the robin lab or clean room, then please create a help desk ticket or email info@lnf.umich.edu. All photoresists must be handled using the green polychloroprene gloves.
  
==Announcements==
+
 
* None at this time.
 
  
 
==Photoresist Table==
 
==Photoresist Table==

Revision as of 10:24, 26 June 2018

Photoresist is a photoactive polymer suspended in a solvent used in Lithography processing. We have positive novolak based resists for use with our mask aligners and stepper, negative epoxy based resists ..... and e-beam resists for use with the JOEL.


LNF Supported Photoresists

...table...

Applications

Etch

  • RIE - Photoresist used in RIE needs to be thermally stable and resistant to the etch chemistry.
  • Wet Etch - A photoresists adhesion is very important as any adhesion failure greatly increases undercut.

Deposition

  • Liftoff - Need a photoresist profile that prevents sidewall deposition. Often this is done by using a bi-layer stack and undercutting the bottom layer.
  • Plating
  • Molding


Below you can find a list of public and private approved photoresists for the LNF. If you would like to bring a new photoresist into the robin lab or clean room, then please create a help desk ticket or email info@lnf.umich.edu. All photoresists must be handled using the green polychloroprene gloves.


Photoresist Table

Photoresists
Photoresist LNF/Private Tool +/-/Reversible Stored Notes
950K PMMA 6% LNF E-Beam Spinner ? Photoresist cabinet 1440C; 1480 photoresist -
AZ5214-E (IR) Private Not using +, Reversible No longer stored -
AZ9260 Sold through store ? + ? Thick photoresist, high resolution
KMPR 1010 Private CEE 100CB Spinner - ? UV, E-beam, x-ray, contact aligner
KMPR 1025 Private CEE 100CB Spinner - ? UV, E-beam, or x-ray
LOR 10B Lift-Off Resist Private CEE 100CB Spinner - ? -
Omni Coat ? ? ? ? -
S1813 LNF CEE 100 and CEE 200 Spinners + Photoresist cabinet 1440C -
SC1827 LNF/discontinued CEE 100 and CEE 200 Spinners + Photoresist cabinet 1440C -
SPR 220-3.0 LNF ACS 200 Cluster Tool, CEE 100 and CEE 200 Spinners + Photoresist cabinet 1440C -
SPR 220-7.0 LNF/Private CEE 100 and CEE 200 Spinners + Photoresist cabinet 1440C LNF provides the photoresist for the CEE 200CB Spinner #1, but it must be purchased if you want to use it on the CEE 100CB Spinner
SPR 955-0.9 LNF ACS 200 Cluster Tool, CEE 100 and CEE 200 Spinners + Photoresist cabinet 1440C Thinner viscosity, higher resolution
SU-8 2010 ? ROBIN Lab - Epoxy photoresist for micromachining
SU-8 2005 ? ROBIN Lab - Epoxy photoresist for micromachining
SU-8 2050 ? ROBIN Lab - Epoxy photoresist for micromachining