Difference between revisions of "Plasmatherm 790"
Line 10: | Line 10: | ||
|maintenance = [https://docs.google.com/a/lnf.umich.edu/document/d/1OvMzJ2QibI7rEU3ApebmoEPh_nvhBoVxd8NIxHiax0U/preview Maintenance Overview] | |maintenance = [https://docs.google.com/a/lnf.umich.edu/document/d/1OvMzJ2QibI7rEU3ApebmoEPh_nvhBoVxd8NIxHiax0U/preview Maintenance Overview] | ||
|processes = [[{{PAGENAME}}/Processes|Supported Processes]] | |processes = [[{{PAGENAME}}/Processes|Supported Processes]] | ||
− | |userprocesses = [[LNF_User:Plasmatherm_790_User_Processes|User Processes]] }} {{warning|This page has not been released yet.}} The Plasmatherm 790 is a dual chamber parallel plate tool. The left chamber is configured for reactive ion etching (RIE) while the right chamber is configured for plasma enhanced chemical vapor deposition (PECVD). The RIE chamber is one of the slower etchers in the lab, especially compared to the [[ | + | |userprocesses = [[LNF_User:Plasmatherm_790_User_Processes|User Processes]] }} {{warning|This page has not been released yet.}} The Plasmatherm 790 is a dual chamber parallel plate tool. The left chamber is configured for reactive ion etching (RIE) while the right chamber is configured for plasma enhanced chemical vapor deposition (PECVD). The RIE chamber is one of the slower etchers in the lab, especially compared to the [[P5000 RIE]]. The main advantage is that there are almost no material restrictions, so a wide variety of materials can be processed. The PECVD is also much slower compared to the [[P5000 PECVD]]; this can actually be advantageous as the smaller building blocks can improve a films quality. |
Revision as of 09:41, 19 May 2015
This article's lead section may not adequately summarize key points of its contents. |
Plasmatherm 790 | |
---|---|
Equipment Details | |
Technology | RIE |
Materials Restriction | Metals |
Material Processed | Si, SiO2 |
Mask Materials | PR, SiO2 |
Gases Used | He, O2, SF6 |
Equipment Manual | |
Overview | System Overview |
Operating Procedure | SOP |
Supported Processes | Supported Processes |
User Processes | User Processes |
Maintenance | Maintenance Overview |
This page has not been released yet. |
The Plasmatherm 790 is a dual chamber parallel plate tool. The left chamber is configured for reactive ion etching (RIE) while the right chamber is configured for plasma enhanced chemical vapor deposition (PECVD). The RIE chamber is one of the slower etchers in the lab, especially compared to the P5000 RIE. The main advantage is that there are almost no material restrictions, so a wide variety of materials can be processed. The PECVD is also much slower compared to the P5000 PECVD; this can actually be advantageous as the smaller building blocks can improve a films quality.
Contents
Announcements
- [2014-09-25] - Added 500 sccm Helium MFC to PECVD chamber.
Capabilities
- Wide variety of materials processed
- Wide variety of gases available
- Generally slower etch rates <1000 Å/min
System Overview
Hardware Details
- RIE Gases
- PECVD Gases
- Pressure
- RIE: 5 - 300 mTorr
- PECVD: 50 - 2000 mTorr
- Chuck
- PECVD: Heated Platen: 200°C - 350°C
- RF
- 400 W 13.56 MHz RF Source
Substrate Requirements
- RIE
- Up to 3 100 mm (4") wafers
- Pieces don't require mounting
- PECVD
- 1 150 mm (6") wafer
- 2 100 mm (4") wafers
- Several pieces
Material Restrictions
This section may need to be rewritten entirely to comply with The LNF wiki's quality standards, as it does not match the boilerplate and it only includes the left chamber. |
Below is a list of approved and restricted materials for the tool. "Approved" means the material is allowed in the tool under normal circumstances. "Not Allowed" means the material may never be used in the tool. If a material is not listed, it may be possible to use the material under certain conditions. Please contact a tool engineer via the helpdesk ticket system for any material requests or questions.
Left Chamber
Supported Processes
This section requires expansion with: the process subpages are incomplete. |
There are several processes for this tool supported by the LNF, which are described in more detail on the Processes page.
In addition to these, this tool has a number of user-created recipes for etching a wide variety of materials. Some of these recipes are documented on LNF User:Plasmatherm 790 User Processes. If you are curious if your material can be processed in this tool, please contact the tool engineers via the helpdesk ticket system.
Standard Operating Procedure
Widget text will go here.
Checkout Procedure
- Read through the Standard Operating Procedure above.
- Complete the training request form here.
- Create a helpdesk ticket requesting training.
- A tool engineer will schedule a time for initial training.
- Practice with your mentor or another authorized user until you are comfortable with tool operation.
- Complete the SOP quiz here.
- Schedule a checkout session with a tool engineer via the helpdesk ticket system. If this checkout is successful, the engineer will authorize you on the tool.
Maintenance
Every other week a light cleaning is performed on the tool. A 5 min etch with m_si_o_1 is performed on a 4" oxide wafer as a qualification run. The results can be seen below.