Line 27: Line 27:
  
 
Then there is also 1 oxynitride recipe at 350°C.  It is designed to have minimal stress.
 
Then there is also 1 oxynitride recipe at 350°C.  It is designed to have minimal stress.
* [[Plasmatherm 790/Processes/L_on350]]
+
* [[Plasmatherm 790/Processes/L_oxy350]]
  
 
There is also DBR_N_O which has 4 deposition steps consisting of L_NIT200,L_OX200,L_NIT200,L_OX200
 
There is also DBR_N_O which has 4 deposition steps consisting of L_NIT200,L_OX200,L_NIT200,L_OX200

Revision as of 10:34, 7 August 2019

This page lists the processes supported by the LNF for the Plasmatherm 790.

Process List

RIE

PECVD

The Plasmatherm has 3 oxide recipes available, at 200°C, and 350°C.

There are also 2 nitride recipes available, at 200°C, and 350°C. These have the index and stress optimized.

Then there is also 1 oxynitride recipe at 350°C. It is designed to have minimal stress.

There is also DBR_N_O which has 4 deposition steps consisting of L_NIT200,L_OX200,L_NIT200,L_OX200