Difference between revisions of "Plasmatherm 790/Processes/m pary1"

From LNF Wiki
Jump to navigation Jump to search
(Created page with "<!-- Make sure to add any other relevant categories --> Category:Processes {{warning|This page has not been released yet.}} {{Infobox process |image = |caption =...")
 
Line 54: Line 54:
  
 
{{#widget:Iframe
 
{{#widget:Iframe
|url=
+
|url=https://docs.google.com/spreadsheets/d/1jDSV00jZ-1vppt2MgGRAJyXRvxEE3rJIlXtngODM9-0/pubchart?oid=1193338187&format=interactive
|width=600
+
|width=700
|height=400
+
|height=350
 +
|border=0
 +
}}
 +
 
 +
Then occasionally the recipe is tested on other materials as shown below.
 +
{{#widget:Iframe
 +
|url=https://docs.google.com/spreadsheets/d/1jDSV00jZ-1vppt2MgGRAJyXRvxEE3rJIlXtngODM9-0/pubchart?oid=1193338187&format=interactive
 +
|width=700
 +
|height=350
 
|border=0
 
|border=0
 
}}
 
}}

Revision as of 13:38, 24 February 2015

Warning Warning: This page has not been released yet.
About this Process
Process Details
Equipment Plasmatherm 790
Technology RIE
Material Parylene
Mask Materials Photoresist
Gases Used O2


m_pary1 is an O2 etch that can be used for parylene and other polymers.

Parameters

Parameter Etch
RF Power 105 W
Pressure 100 mTorr
O2 Flow 99 sccm

Capabilities

Etch Rate

Mask Selectivity

Sidewall Profile

  • Undercut: XXX


Limitations

????

Qualification

Once a month m_pary1 is run on a XXX. This etch rate is reported in the chart below.

Then occasionally the recipe is tested on other materials as shown below.