Difference between revisions of "Plasmatherm 790/Processes/m pary1"

From LNF Wiki
Jump to navigation Jump to search
Line 38: Line 38:
  
 
===Mask Selectivity===
 
===Mask Selectivity===
* [[Silicon Dioxide|SiO2]] Etch Rate: XXX
+
* [[Silicon Dioxide|SiO2]] Etch Rate: <5  Å/min
 
* Photoresist Etch Rate
 
* Photoresist Etch Rate
 
** [[SPR 220]]: XXX
 
** [[SPR 220]]: XXX

Revision as of 13:39, 24 February 2015

Warning Warning: This page has not been released yet.
About this Process
Process Details
Equipment Plasmatherm 790
Technology RIE
Material Parylene
Mask Materials Photoresist
Gases Used O2


m_pary1 is an O2 etch that can be used for parylene and other polymers.

Parameters

Parameter Etch
RF Power 105 W
Pressure 100 mTorr
O2 Flow 99 sccm

Capabilities

Etch Rate

Mask Selectivity

  • SiO2 Etch Rate: <5 Å/min
  • Photoresist Etch Rate

Sidewall Profile

  • Undercut: XXX


Limitations

????

Qualification

Once a month m_pary1 is run on a XXX. This etch rate is reported in the chart below.

Then occasionally the recipe is tested on other materials as shown below.